Nylon 11 . 12 - PA11.12


Molding Properties
    ·    Drying temperature                                : 70~80°C
    ·    Drying time                                            : 8~15hr
    ·    Injection forming cylinder temperature    : 190~270°C
    ·    Injection molding tool temperature          : 20~100°C
    ·    Injection molding pressure                      : —
    ·    Compression molding temperature          : —
    ·    Compression molding pressure               : —
    ·    Molding shrinkage rate                           : 0.3~1.5%
    ·    Specific gravity                                      : 1.03~1.08density
       JIS : K6911,K7122
       A.S.T.M   : D792


Mechanical Characteristics
    ·    Tensile strength                 : 530~550kgf/cm2
       JIS : K6911,K7113
       A.S.T.M   : D638
    ·    Tensile elongation               : 300~500%
    ·    Compressive strength         : —
       JIS : K7208
    ·    Flexure strength                 : —
       JIS : K7203
    ·    Izot impact strength            : 10~30kgf/cm2
       JIS : K7110,K7111
    ·    Rockwell hardness             : R106~109
       JIS : K7202
       A.S.T.M   : D785


Thermal Characteristic
    ·    Heat resistance temperature (continuous)    : 82~149°C
    ·    Deflection temperature under load
         a) Bending stress18.6kgf/cm2                     : 54.2°C
         b) Bending stress 4.6kgf/cm2                      : 167°C
       JIS : K7206,K7207
       A.S.T.M   : D648